Kinga Kowalska Art / river table / 5 cm

Deep Pour (River Table up to 5 cm)

Product card with pour depth, curing time, mix ratio and practical workshop guidance from the NeuroResin database.

crystal clear (self-leveling, self-degassing) deep cast high (stabilizator HALS) ratio 100:40

About the product

Deep Pour (River Table up to 5 cm) by Kinga Kowalska Art is a deep cast epoxy resin for river table work, with a maximum working layer of 5 cm. The database records a 100:40 mix ratio, working time around 1 h (60 min), transparency described as crystal clear (self-leveling, self-degassing), UV resistance: high (stabilizator HALS) and viscosity: low (wodnista konsystencja). Full cure is listed as 14 days (336 h), so mechanical work should be planned with a safety margin rather than only around demolding time.

Working with it

For Deep Pour (River Table up to 5 cm), the key is calm setup and process control. Work at a stable temperature around 18-23C; in colder conditions this resin may cure more slowly, turn cloudy or remain soft on the surface. Keep the 100:40 ratio and mix slowly but thoroughly; with this resin class, poor mixing causes problems more often than the product itself. For wood and porous substrates, apply a seal coat before the main pour. The 5 cm layer limit should not be treated as extra safety margin when the mass is high, the mold is closed or the workshop is warm. Use the two-cup method: after the first mix, transfer into a second cup and mix again to reduce streaks and soft spots from the cup walls.

Summary

Deep Pour (River Table up to 5 cm) is best treated as a product for projects where the layer limit, patient degassing and full cure time of 14 days (336 h) matter. Choose a finish according to exposure, abrasion and expected sheen. Before the final pour, make a small sample using the target wood, pigment and workshop temperature.

Database parameters

Classdeep cast
Ratio100:40
Demold2 days (48 h)
Full cure14 days (336 h)

Working tips

Work at a stable temperature around 18-23C; in colder conditions this resin may cure more slowly, turn cloudy or remain soft on the surface.
Keep the 100:40 ratio and mix slowly but thoroughly; with this resin class, poor mixing causes problems more often than the product itself.
Use the two-cup method: after the first mix, transfer into a second cup and mix again to reduce streaks and soft spots from the cup walls.

Product FAQ

What is the maximum layer for Kinga Kowalska Art Deep Pour (River Table up to 5 cm)?

The NeuroResin database lists the maximum working layer as 5 cm. For larger masses, warmer workshops or closed molds, keep a safety margin.

What is the working time of Kinga Kowalska Art Deep Pour (River Table up to 5 cm)?

The listed working time is about 1 h (60 min). It depends on temperature, mixed mass and pour geometry.

When does Kinga Kowalska Art Deep Pour (River Table up to 5 cm) reach full cure?

Full cure is listed as 14 days (336 h). Demolding may be possible earlier, around 2 days (48 h), but machining is best planned after full cure.

Purchase

This resin record does not currently include a public purchase link.

This resin product card is generated from NeuroResin product parameters and working notes. Always verify the current manufacturer TDS/SDS before production.